Common Trade Name |
A286 |
|
Material Grade |
A286 |
|
UNS |
S66286 |
|
Specification |
ASTM A453 |
|
Approx. Room Temp.
Mechanicals |
"T = 130 ksi, Y = 85 ksi" |
|
Typical % Composition
Summary |
"Ni 25.5, Fe 56.5, Cr
15, Ti 2.1, Mo 1.25" |
|
Applications |
"Used for high strength
and corrosion resistance up to 700 deg
C (approx)." |
|
Corrosion Resistance |
"Iron base, heat and corrosion
resistant, austenitic alloy. Also used
for low temperature applications exhibiting
good ductility, high strength and non
-magnetic features at room temp to -196
deg C." |
| back to materials main menu | |
|
|
|