Common Trade Name |
347 |
|
Material Grade |
347 |
|
UNS |
S34700 |
|
Specification |
A193 B8C |
|
Approx. Room Temp.
Mechanicals |
"T = 75 ksi, Y = 30 ksi" |
|
Typical % Composition
Summary |
"Ni 9, Cr 18, Mn 2max,
C .08max, Cb 10 x C" |
|
Applications |
"Primarily used by aircraft
industry. Used where intermittent exposure
to temperatures above 800 deg F occurs." |
|
Corrosion Resistance |
"Stabilized stainless
offering excellent resistance to intergranular
corrosion following temperatures in the
chromium carbide precipitation range from
800 to 1500 deg C. The addition of columbium
and tantalum stabilize against chromium
carbide formation. " |